Heat treatment to reduce the susceptibility of Al-Zn-Mg-Cu alloy to stress corrosion cracking.
OHNISHI, Tadakazu, SHIOTA, HideakiVolume:
36
Year:
1986
Language:
english
Journal:
Journal of Japan Institute of Light Metals
DOI:
10.2464/jilm.36.647
File:
PDF, 1.99 MB