![](/img/cover-not-exists.png)
Effects of Alloying Additions on the Creep Strength of a Fourth Generation Single-Crystal Superalloy
Koizumi, Yutaka, Kobayashi, Toshiharu, Yokokawa, Tadaharu, Osawa, Makoto, Harada, Hiroshi, Aoki, Yasuhiro, Arai, MikiyaVolume:
68
Year:
2004
Language:
english
Journal:
Journal of the Japan Institute of Metals
DOI:
10.2320/jinstmet.68.206
File:
PDF, 1.85 MB
english, 2004