Mechanical Properties of Cast & Wrought Pancakes Using New Ni-Co Base Disk Superalloys
Yokokawa, Tadaharu, Gu, Yuefeng, Cui, Chuanyong, Koizumi, Yutaka, Fujioka, Junzo, Harada, Hiroshi, Fukuda, Tadashi, Mitsuhashi, AkiraVolume:
74
Year:
2010
Language:
english
Journal:
Journal of the Japan Institute of Metals