Atomic layer deposition of NiS and its application as cathode material in dye sensitized solar cell
Mahuli, Neha, Sarkar, Shaibal K.Volume:
34
Language:
english
Journal:
Journal of Vacuum Science & Technology A: Vacuum, Surfaces, and Films
DOI:
10.1116/1.4938078
Date:
January, 2016
File:
PDF, 1.86 MB
english, 2016