![](/img/cover-not-exists.png)
Study of the surface size defects in the case of a soda lime glass eroded by sandblasting
Faci, A., Kolli, M., Bouaouadja, N., Chabane, B., El Bouari, A., El Ouatib, R., Hannache, H., Krimi, S., Lamire, M., Mansouri, I., Moussa, R., Aboulayt, A.Volume:
5
Year:
2013
Language:
english
Journal:
MATEC Web of Conferences
DOI:
10.1051/matecconf/20130504038
File:
PDF, 219 KB
english, 2013