Influence of nitrogen addition on microstructure and pitting corrosion resistance of austenitic weld metals
Mudali, U. Kamachi, Dayal, R. K., Gill, T. P. S., Gnanamoorthy, J. B.Volume:
37
Language:
english
Journal:
Materials and Corrosion
DOI:
10.1002/maco.19860371206
Date:
December, 1986
File:
PDF, 1.97 MB
english, 1986