![](/img/cover-not-exists.png)
Development of the recovery technology for nickel superalloy blades of the aircraft engine by laser cladding
Bykovskiy, D P, Petrovskiy, V N, Polskiy, V I, Chirikov, S N, Dzhumaev, P SVolume:
747
Language:
english
Journal:
Journal of Physics: Conference Series
DOI:
10.1088/1742-6596/747/1/012056
Date:
September, 2016
File:
PDF, 1.13 MB
english, 2016