![](/img/cover-not-exists.png)
Reference material for temperature calibration of differential scanning calorimeters above 1400 °C
Zorzi, J. E., Segadães, A. M., Perottoni, C. A.Language:
english
Journal:
Journal of Thermal Analysis and Calorimetry
DOI:
10.1007/s10973-016-6048-8
Date:
December, 2016
File:
PDF, 1.36 MB
english, 2016