![](/img/cover-not-exists.png)
Microchannel plate fabrication using glass capillary arrays with Atomic Layer Deposition films for resistance and gain
Popecki, M. A., Adams, B., Craven, C. A., Cremer, T., Foley, M. R., Lyashenko, A., O'Mahony, A., Minot, M. J., Aviles, M., Bond, J. L., Stochaj, M. E., Worstell, W., Elam, J. W., Mane, A. U., SiegmundVolume:
121
Language:
english
Journal:
Journal of Geophysical Research: Space Physics
DOI:
10.1002/2016JA022580
Date:
August, 2016
File:
PDF, 2.82 MB
english, 2016