Mechanical properties examined by nanoindentation for selected phases relevant to the development of monolithic uranium-molybdenum metallic fuels
Newell, Ryan, Park, Youngjoo, Mehta, Abhishek, Keiser, Dennis, Sohn, YonghoVolume:
487
Language:
english
Journal:
Journal of Nuclear Materials
DOI:
10.1016/j.jnucmat.2017.02.018
Date:
April, 2017