![](/img/cover-not-exists.png)
Limits of applicability of the temperature/work-of-rupture relationships and micro fractography in estimating the brittle-tough transition of steels
O. N. Romaniv, M. A. Kutsyn, Yu. D. Petrina, Yu. V. ZimaVolume:
10
Language:
english
Pages:
7
DOI:
10.1007/bf01149500
Date:
March, 1974
File:
PDF, 935 KB
english, 1974