Frequency-dependent attenuation in water-saturated cracked glass based on creep tests
Mallet, Céline, Quintal, Beatriz, Caspari, Eva, Holliger, KlausVolume:
82
Language:
english
Journal:
GEOPHYSICS
DOI:
10.1190/geo2016-0142.1
Date:
May, 2017