![](/img/cover-not-exists.png)
Toward ultrafast lithium ion capacitors: A novel atomic layer deposition seeded preparation of Li 4 Ti 5 O 12 /graphene anode
Wang, Gongkai, Lu, Chengxing, Zhang, Xin, Wan, Biao, Liu, Hanyu, Xia, Meirong, Gou, Huiyang, Xin, Guoqing, Lian, Jie, Zhang, YongguangVolume:
36
Language:
english
Journal:
Nano Energy
DOI:
10.1016/j.nanoen.2017.04.020
Date:
June, 2017
File:
PDF, 3.43 MB
english, 2017