![](/img/cover-not-exists.png)
The Application of Rough Sets Theory to Design of Weld Defect Classifiers
Chady, Tomasz, Sikora, Ryszard, Misztal, Leszek, Grochowalska, Barbara, Grzywacz, Bogdan, Szydłowski, Michał, Waszczuk, Paweł, Szwagiel, MariuszVolume:
36
Language:
english
Journal:
Journal of Nondestructive Evaluation
DOI:
10.1007/s10921-017-0420-x
Date:
June, 2017
File:
PDF, 923 KB
english, 2017