Mechanical characterization via nanoindentation of the woven bone developed during bone transport
Mora-Macías, J., Pajares, A., Miranda, P., Domínguez, J., Reina-Romo, E.Volume:
74
Language:
english
Journal:
Journal of the Mechanical Behavior of Biomedical Materials
DOI:
10.1016/j.jmbbm.2017.05.031
Date:
October, 2017