Effects of Cutting Parameters over Turning of UDIMET ® 720 Superalloy in a Broaching Process Simulation
Bonnardel, Quentin, Wagner, Vincent, Dessein, Gilles, Dutilh, Vincent, Mandrile, SebastienVolume:
58
Year:
2017
Language:
english
Journal:
Procedia CIRP
DOI:
10.1016/j.procir.2017.03.323
File:
PDF, 453 KB