![](/img/cover-not-exists.png)
Experimental study of fibre laser microdrilling of aerospace superalloy by trepanning technique
Tagliaferri, F., Genna, S., Leone, C., Palumbo, B., De Chiara, G.Language:
english
Journal:
The International Journal of Advanced Manufacturing Technology
DOI:
10.1007/s00170-017-0773-4
Date:
July, 2017
File:
PDF, 3.18 MB
english, 2017