![](/img/cover-not-exists.png)
X-ray Inspection of MIM 418 Superalloy Turbine Wheels and Defects Analysis
Yanhong, Jing, Fubao, Yang, Daquan, Li, Hao, Li, Lin, Zhang, Dan, Li, Qiang, ZhuVolume:
46
Language:
english
Journal:
Rare Metal Materials and Engineering
DOI:
10.1016/S1875-5372(17)30087-5
Date:
February, 2017
File:
PDF, 696 KB
english, 2017