![](/img/cover-not-exists.png)
Investigation of the fracture of very thin amorphous alumina film during spherical nanoindentation
Mercier, David, Mandrillon, Vincent, Parry, Guillaume, Verdier, Marc, Estevez, Rafael, Bréchet, Yves, Maindron, TonyVolume:
638
Language:
english
Journal:
Thin Solid Films
DOI:
10.1016/j.tsf.2017.07.040
Date:
September, 2017
File:
PDF, 3.83 MB
english, 2017