![](/img/cover-not-exists.png)
Extending the service life of pipelines with weld defects
Yu Latypova, E., Tsumarev, Yu. A., Klochkov, V. N.Volume:
31
Language:
english
Journal:
Welding International
DOI:
10.1080/09507116.2017.1353277
Date:
December, 2017
File:
PDF, 667 KB
english, 2017