Studies on poly(ethylene terephthalate)/cotton blends by differential scanning calorimetry
B. Basak, O. Okpe, S. C. O. UgbolueVolume:
21
Language:
english
Pages:
10
DOI:
10.1007/bf01914207
Date:
August, 1981
File:
PDF, 443 KB
english, 1981