Effects of scanning speed on microstructure in laser surface-melted single crystal superalloy and theoretical analysis
Wang, Guowei, Liang, Jingjing, Yang, Yanhong, Shi, Yu, Zhou, Yizhou, Jin, Tao, Sun, XiaofengLanguage:
english
Journal:
Journal of Materials Science & Technology
DOI:
10.1016/j.jmst.2017.11.027
Date:
November, 2017