![](/img/cover-not-exists.png)
Elemental preference and atomic scale site recognition in a Co-Al-W-base superalloy
Chen, Yanhui, Xue, Fei, Mao, Shengcheng, Long, Haibo, Zhang, Bin, Deng, Qingsong, Chen, Bin, Liu, Yinong, Maguire, Pierce, Zhang, Hongzhou, Han, Xiaodong, Feng, QiangVolume:
7
Language:
english
Journal:
Scientific Reports
DOI:
10.1038/s41598-017-17456-1
Date:
December, 2017
File:
PDF, 2.65 MB
english, 2017