![](/img/cover-not-exists.png)
Enhanced wear resistance of laser cladded graphene nanoplatelets reinforced Inconel 625 superalloy composite coating
Deng, Pingshun, Yao, Chengwu, Feng, Kai, Huang, Xiangxiang, Li, Zhuguo, Li, Yuyan, Zhao, HaixingVolume:
335
Language:
english
Journal:
Surface and Coatings Technology
DOI:
10.1016/j.surfcoat.2017.12.047
Date:
February, 2018
File:
PDF, 2.71 MB
english, 2018