8th International Symposium on Superalloy 718 and Derivatives (Ott/8th International) || Hold Time Effects on the Crack Growth Behavior in Inco 718 Alloy
Ott, Eric, Banik, Anthony, Andersson, Joel, Dempster, Ian, Gabb, Tim, Groh, Jon, Heck, Karl, Helmink, Randy, Liu, Xingbo, Wusatowska-Sarnek, AgnieszkaVolume:
10.1002/97
Year:
2014
Language:
english
DOI:
10.1002/9781119016854.ch42
File:
PDF, 1.02 MB
english, 2014