Core structure and strengthening mechanism of the misfit dislocation in nickel-based superalloys during high-temperature and low-stress creep
Ma, Shiyu, Lv, Xianzi, Zhang, Jianxin, Zhang, Youjian, Li, Pan, Jin, Huixin, Zhang, Wenyang, Li, Xueqiao, Mao, ShengchengLanguage:
english
Journal:
Journal of Alloys and Compounds
DOI:
10.1016/j.jallcom.2018.01.323
Date:
January, 2018
File:
PDF, 6.50 MB
english, 2018