![](/img/cover-not-exists.png)
Multi-temperature indentation creep tests on nanotwinned copper
Yang, Xu-Sheng, Zhai, Hui-Ru, Ruan, Hai-Hui, Shi, San-Qiang, Zhang, Tong-YiLanguage:
english
Journal:
International Journal of Plasticity
DOI:
10.1016/j.ijplas.2018.01.016
Date:
February, 2018
File:
PDF, 1.64 MB
english, 2018