![](/img/cover-not-exists.png)
Correlation between evolution of inclusions and pitting corrosion in 304 stainless steel with yttrium addition
Shi, Weining, Yang, Shufeng, Li, JingsheVolume:
8
Language:
english
Journal:
Scientific Reports
DOI:
10.1038/s41598-018-23273-x
Date:
December, 2018
File:
PDF, 2.34 MB
english, 2018