![](/img/cover-not-exists.png)
Thermal dynamic behavior during selective laser melting of K418 superalloy: numerical simulation and experimental verification
Chen, Zhen, Xiang, Yu, Wei, Zhengying, Wei, Pei, Lu, Bingheng, Zhang, Lijuan, Du, JunVolume:
124
Language:
english
Journal:
Applied Physics A
DOI:
10.1007/s00339-018-1737-8
Date:
April, 2018
File:
PDF, 4.45 MB
english, 2018