Fatigue Crack Initiation in Nickel-Based Superalloy MAR-M247 at High Temperature
Šulák, Ivo, Obrtlík, KarelVolume:
754
Language:
english
Journal:
Key Engineering Materials
DOI:
10.4028/www.scientific.net/KEM.754.27
Date:
September, 2017
File:
PDF, 2.19 MB
english, 2017