![](/img/cover-not-exists.png)
The Effects of Dissolved Oxygen Concentration and Temperature on the Stress Corrosion Cracking of Low Alloy Steels in High Temperature Water
Kuniya, Jiro, Kanno, Masayoshi, Masaoka, Isao, Sasaki, RyoichiVolume:
32
Year:
1983
Journal:
CORROSION ENGINEERING
DOI:
10.3323/jcorr1974.32.11_649
File:
PDF, 2.93 MB
1983