![](/img/cover-not-exists.png)
Observation of Pitting Corrosion of Stainless Steels in Chloride Solutions by Random Pulse Method
Motooka, Takafumi, Sugie, Yosohiro, Kobune, Masafumi, Fujii, SatoshiVolume:
42
Year:
1993
Journal:
Zairyo-to-Kankyo
DOI:
10.3323/jcorr1991.42.93
File:
PDF, 711 KB
1993