![](/img/cover-not-exists.png)
Effects of Potential and Concentration of Bicarbonate Solution on Stress Corrosion Cracking of Annealed Carbon Steel
Haruna, Takumi, Zhu, Liehong, Murakami, Makoto, Shibata, ToshioVolume:
49
Year:
2000
Language:
english
Journal:
Zairyo-to-Kankyo
DOI:
10.3323/jcorr1991.49.144
File:
PDF, 3.79 MB
english, 2000