Study on the Mechanism of Intergranular Stress Corrosion Cracking of Alloy 600 in High Temperature Alkaline Solution
Kawamura, Hirotaka, Hirano, Hideo, Takamatsu, Hiroshi, Matsunaga, Tomoya, Shirai, Shunsuke, Yamaoka, Katsuaki, Ohshinden, Kimihisa, Sakai, KimioVolume:
48
Year:
1999
Language:
english
Journal:
Zairyo-to-Kankyo
DOI:
10.3323/jcorr1991.48.226
File:
PDF, 3.67 MB
english, 1999