Fermi Level Tuning of ZnO Films Through Supercycled Atomic Layer Deposition
Huang, Ruomeng, Ye, Sheng, Sun, Kai, Kiang, Kian S., de Groot, C. H.Volume:
12
Language:
english
Journal:
Nanoscale Research Letters
DOI:
10.1186/s11671-017-2308-1
Date:
December, 2017
File:
PDF, 1.76 MB