![](/img/cover-not-exists.png)
Advanced 3D characterisation of iodine induced stress corrosion cracks in zirconium alloys
Gillen, Conor, Garner, Alistair, Plowman, Adam, Race, Christopher P., Lowe, Tristan, Jones, Christopher, Moore, Katie L., Frankel, PhilippVolume:
141
Language:
english
Journal:
Materials Characterization
DOI:
10.1016/j.matchar.2018.04.034
Date:
July, 2018
File:
PDF, 4.27 MB
english, 2018