![](/img/cover-not-exists.png)
Quantitative characterization of nanoindentation properties of CVI gradient SiC ceramic into CNT arrays
Mei, Hui, Kong, Ziyan, Xia, Junchao, Cheng, Laifei, Jiang, Kaili, Fan, ShoushanVolume:
762
Language:
english
Journal:
Journal of Alloys and Compounds
DOI:
10.1016/j.jallcom.2018.05.185
Date:
September, 2018
File:
PDF, 3.40 MB
english, 2018