Influence of surface modifications by laser shock processing on the acid chloride stress corrosion cracking susceptibility of AISI 304 stainless steel
Wei, Xinlong, Ling, Xiang, Zhang, MengVolume:
91
Language:
english
Journal:
Engineering Failure Analysis
DOI:
10.1016/j.engfailanal.2018.04.045
Date:
September, 2018
File:
PDF, 1.55 MB