![](/img/cover-not-exists.png)
ChemInform Abstract: ELECTROCHEMICAL INVESTIGATIONS OF PITTING CORROSION
HERBSLEB, GUENTER, SCHWENK, WILHELMVolume:
4
Journal:
Chemischer Informationsdienst
DOI:
10.1002/chin.197352036
Date:
December, 1973
File:
PDF, 120 KB
1973