Development of Transient Liquid Phase Bonding of Ni-base Superalloy, Inconel 718 to Skip Homogenising Heat Treatment
SAKAMOTO, Rie, NAKANISHI, Takeo, SAIDA, Kazuyoshi, NISHIMOTO, KazutoshiVolume:
24
Year:
2006
Journal:
QUARTERLY JOURNAL OF THE JAPAN WELDING SOCIETY
DOI:
10.2207/qjjws.24.273
File:
PDF, 817 KB
2006