![](/img/cover-not-exists.png)
Stress Corrosion Cracking Behavior of Fine-Grained AZ61 Magnesium Alloys Processed by Equal-Channel Angular Pressing
Xie, Qiuyuan, Ma, Aibin, Jiang, Jinghua, Cheng, Zhaojun, Song, Dan, Yuan, Yuchun, Liu, HuanVolume:
7
Language:
english
Journal:
Metals
DOI:
10.3390/met7090343
Date:
September, 2017
File:
PDF, 4.33 MB
english, 2017