![](/img/cover-not-exists.png)
Tensile and Creep Testing of Sanicro 25 Using Miniature Specimens
Dymáček, Petr, Jarý, Milan, Dobeš, Ferdinand, Kloc, LubošVolume:
11
Language:
english
Journal:
Materials
DOI:
10.3390/ma11010142
Date:
January, 2018
File:
PDF, 32.92 MB
english, 2018