Investigations into the Surface Strain/Stress State in a Single-Crystal Superalloy via XRD Characterization
Duan, Haodong, Qin, Lu, Pei, Yanling, Li, Shusuo, Zhao, Li-Dong, Ji, Vincent, Gong, ShengkaiVolume:
8
Language:
english
Journal:
Metals
DOI:
10.3390/met8060376
Date:
May, 2018
File:
PDF, 3.28 MB
english, 2018