Atmospheric spatial atomic layer deposition of ZnOS buffer layers for flexible Cu(In,Ga)Se 2 solar cells
Illiberi, Andrea, Frijters, Corne, Ruth, Marta, Bremaud, David, Poodt, Paul, Roozeboom, Fred, Bolt, Pieter JanVolume:
36
Language:
english
Journal:
Journal of Vacuum Science & Technology A
DOI:
10.1116/1.5040457
Date:
September, 2018