Effects of Aging at 450°C on the Pitting Corrosion Resistance and Toughness of AISI 317L Steel Welded by GTAW and FSW
Farneze, Humberto Nogueira, Tavares, Sérgio Souto Maior, Pardal, Juan Manuel, Barbosa, Cássio, Pereira, Olívia Cypreste, Cunha, Rachel Pereira Carneiro daVolume:
20
Language:
english
Journal:
Materials Research
DOI:
10.1590/1980-5373-mr-2016-1007
Date:
November, 2017