Identification of Constitutive Model Parameters for Nimonic 80A Superalloy
Korkmaz, Mehmet Erdi, Verleysen, Patricia, Günay, MustafaLanguage:
english
Journal:
Transactions of the Indian Institute of Metals
DOI:
10.1007/s12666-018-1394-9
Date: