Local structure and point defects-dependent Area-Selective Atomic Layer Deposition Approach for Facile Synthesis of p-Cu2O/n-ZnO Segmented Nano-junctions
de Melo Sánchez, Claudia, Jullien, Maud, Ghanbaja, Jaafar, Montaigne, François, Pierson, Jean Francois, Soldera, Flavio, Rigoni, Federica, Almqvist, Nils, Vomiero, Alberto, Mücklich, Frank, Horwat, DaLanguage:
english
Journal:
ACS Applied Materials & Interfaces
DOI:
10.1021/acsami.8b12584
Date:
September, 2018
File:
PDF, 2.73 MB
english, 2018