![](/img/cover-not-exists.png)
Occurrence of Near-Neutral pH Stress Corrosion Cracking in X80 and X100 Pipe Steels Under Various Cathodic Protection Conditions
Yan, Li, Gravel, Jean-Philippe, Kang, Jidong, Xu, Luyao, Arafin, MuhammadVolume:
74
Language:
english
Journal:
CORROSION
DOI:
10.5006/2715
Date:
September, 2018
File:
PDF, 1.63 MB
english, 2018