Tensile mechanical properties and fracture behaviors of nickel-based superalloy 718 in the presence of hydrogen
Li, Xinfeng, Zhang, Jin, Fu, Qinqin, Akiyama, Eiji, Song, Xiaolong, Wang, Yanfei, Li, Qizhen, Zou, NingLanguage:
english
Journal:
International Journal of Hydrogen Energy
DOI:
10.1016/j.ijhydene.2018.08.179
Date:
October, 2018