Effect of Pigging Damage on Sulfide Stress Corrosion Cracking of Type 316L Stainless Steel Cladding
Hesketh, J., Hinds, G., Morana, R.Volume:
74
Language:
english
Journal:
CORROSION
DOI:
10.5006/2621
Date:
April, 2018
File:
PDF, 1.24 MB
english, 2018